Ben Brockert wrote:
> On Mon, Oct 14, 2013 at 5:01 PM, George Herbert
> <george.herbert@xxxxxxxxx> wrote:
>> 2024 is SCC sensitive?  Or did you have another alloy in mind?
> 
> "Alloys 7079-T6, 7075 -T6 and 2024 - T3 contributed to more than 90%
> of the service failures of all high-strength aluminum alloys."

Don't these alloys, between them, represent most of the in-service
population of "high-strength aluminum alloys"?

It seems they might collect "90% of the service failures" just from
those statistics (independent of any particular fragility)...

-dave w